CC2 Sintered Ceramic Sand

  • zgxc

  • Feb 05,2023 00:46:28

  • 0

Detailed introduction

Refractoriness℃

Heat resistance① Sieve pass

rate %

Bulk density g/cm3

 

Air Permeability②

Thermal expansion rate %

1800

90

1.48

310

-0.06

①Temperature maintained at 1,500 °C for 10 minutes, vibrate the screen with aperture 3.35mm for 1 minute, and measure the pass rate;

②particle size test of 50/100.

Features

1.Low crushing rate, low abrasion rate, reduce solid waste emission;

2.Long high-temperature heat-resistant time after coating, reducing sand sticking and sintering phenomenon in castings;

3.Low thermal conductivity, low thermal expansion, which helps to improve the dimensional accuracy of castings;

4.Low angular coefficient, rounded grain shape, higher strength than other materials under the same conditions, and good air permeability.

Product application